11. What is the pre-heat temperature for carbon steel above 19.05MM thk?
Pre – heat temperature for carbon steel above 19.05 mm is 80C.
12. Is post heating required for carbon steel material above 19.05MM thk?
No, post heating is not required for carbon steel material of any thickness.
13. What is the soaking temperature during stress reliving for carbon steel material?
Soaking temperature for carbon steel material during stress reliving is 620C. (20C)
14. What is the soaking period during stress reliving for carbon steel material?
Soaking period for carbon steel material during stress reliving is 1hr.
15. What is the rate of heating & cooling during stress reliving for carbon steel material?
The rate of heating & cooling for carbon steel material during stress reliving is 150c/hr.
16. What is the pre-heat temperature during stress reliving for alloy steel materials?
Pre – heat temperature for AS materials is 180C.
17. What is the soaking temperature during stress reliving for alloy steel material?
Soaking temperature for alloy steel material is 720C(20C).
18. What is the soaking period during stress reliving for alloy steel material?
Soaking period for alloy steel material is 2hrs.
19. What is the rate of heating & cooling during stress reliving for alloy steel material?
The rate of heating & cooling for alloy steel material is 100C/hr.
20. What is the post heat temperature for alloy steel material?
Post heat temperature for alloy steel material is 300C.
About Oilandgasclub.com
Oilandgasclub.com is an international oil and gas (online & offline) conference technical training org from India. Oilandgasclub.com 3000+ professionals trained 150,000 hours of classes delivered 500+ expert trainers available and 3600+ respondents 30+ countries 80+ team. Blogs about technical tips at this blog. Contact or more about customized technical training from this page
70+ courses 7 venues 5 categories
OILANDGASCLUB.COM HAS PUBLISHED 150+ ARTICLES IN THIS BLOG Subscribe
fantastic💪